Typical physical property data, subject to batch test reports.

NO.Test itemsUnitStandardTypical Value
1Tensile strengthMPa≥10.011.5
2Elongation at break point%≥150175
3Volume electrical resistivity @20℃Ω·m≥1.0×10¹²3.5×10¹²
4Limit oxygen index(LOI)%≥3538
5Hot pressure test@90℃%≤5020
6Thermal oven-aged @110℃×168h
The retaining of Tensile strength%≤±20+5
The retaining of elongation%≤±20-5
7Impact Brittleness Temperature@-40℃-0/300/30
8The environmental properties of burned material
8.1The acid gasmg/g≤5.01.0
8.2pH of gas solution——≥4.36.1
8.3Conductivity of gas solutionus/mm≤10.01.2
9Environmental required-Conformed to RoHS、REACH
10Densityg/cm³≤1.601.47
11Hardness Shore A 15SecondShore A93±395
⚠️ Data should not be specification work. In case of colored products, the values could vary slightly by color.
Recommended

Extrusion Process

Note: The temperature for cable extrusion should be set at the situation of good cable surface performance.

Zone1Zone2Zone3Zone4NeckDieEye
110±5℃125±5℃145±5℃155±5℃160±5℃160±5℃160±5℃
Packaging & Storage

Packaging and storage

1

Storage

  • Package: 25kg per bag, Alumni-plastic inner, Kraft paper outside.
  • Storage: no rain, no direct sunlight. Dry it at 60℃ ~ 70℃ about 4 hours if the material was storage more than 3 months before used.
2

Suggestion for processing

  • The compression value of extrusion screw should be 1.2~2.0
  • The time of material heated in the barrel should not exceed 10mins, or it maybe decomposed.