Technical Data
Technical Specifications
Typical physical property data, subject to batch test reports.
| Item | Unit | EHH | EHM | EHL |
|---|---|---|---|---|
| Density | g/cm³ | 0.950~0.978 | 0.940~0.955 | ≤0.940 |
| Melt Index | g/10min | ≤2.0 | ≤2.0 | ≤2.0 |
| Tensile Strength | MPa | ≥20.0 | ≥17.0 | ≥14.0 |
| Elongation at Break | % | ≥650 | ≥600 | ≥600 |
| Low Temperature Brittle Temperature | ℃ | ≤-76 | ≤-76 | ≤-76 |
| Air Aging Condition - Tensile Strength | % | ≥20 | ≥16 | ≥13 |
| Air Aging Condition - Elongation at Break | % | ≥650 | ≥500 | ≥500 |
| Vicat Softening Point | ℃ | ≥110 | --- | --- |
| Resistance to Environmental Stress Cracking F0 | h | ≥500 | ≥500 | ≥500 |
| 20℃ Volume Resistivity | Ω·m | ≥1.0×10¹⁴ | ≥1.0×10¹⁴ | ≥1.0×10¹⁴ |
| 20℃ Dielectric Strength,50Hz | MV/m | ≥25.0 | ≥25.0 | ≥25.0 |
| 20℃ Dielectric Constant,50Hz | / | ≤2.75 | ≤2.75 | ≤2.80 |
| Carbon Black Content | % | 2.60±0.25 | 2.60±0.25 | 2.60±0.25 |
| Carbon Black Dispersion | Grade | ≤3 | ≤3 | ≤3 |
| 200 ℃ Oxidation Induction Time | min | ≥30 | ≥30 | ≥30 |
Recommended
Extrusion Process
Recommend to process with the PE extruder with L/D is more than 25.
| Grade | Machine Barrel Temperature | Molding Temperature |
|---|---|---|
| YHS-EHH | 150-210℃ | 220-230℃ |
| YHS-EHM | 150-210℃ | 210-220℃ |
| YHS-EHL | 150-190℃ | 190-210℃ |