Technical Data
Technical Specifications
Typical physical property data, subject to batch test reports.
| NO. | Test items | Unit | Standard | Typical Value | Test Methods |
|---|---|---|---|---|---|
| 1 | Tensile strength | MPa | ≥25 | 26 | ISO572-2 |
| 2 | Elongation at break point | % | ≥700 | 850 | |
| 3 | Volume electrical resistivity @20 ℃ | Ω·cm | ≥1.0×10¹⁶ | 8.5×10¹⁷ | IEC 60502 |
| 4 | Dielectric strength | kV/mm | ≥25 | 39 | IEC 60243 |
| 5 | MFR@190 ℃×2.16kg | g/10min | ≤2.0 | 0.5 | IEC60093 |
| 6 | Thermal stress @115 ℃×6h | % | ≤10 | 1.5 | IEC60811-508 |
| 7 | Low-temperature embrittlement temperature @ -76 ℃ | ℃ | -76 | Pass | ASTM D746 |
| 8 | ESCR(50 ℃,Igepal 10%,F0) | h | ≥5000 | Pass | IEC60811-406 |
| 9 | Carbon black content | % | 2.60 ±0.25 | 2.61 | IEC60811-605 |
| 10 | Carbon black dispersion | Grade | ≤3 | Pass | ISO 18553 |
| 11 | Oxidation induction period at 200 ℃ | min | ≥30 | Pass | IEC60811-509 |
| 12 | Density | g/cm³ | 0.965 ±0.05 | 0.965 | GB/T1033-1986 |
| 13 | Hardness Shore D 15Second | Shore D | 61 ±3 | 60 | GB2411-1980 |
⚠️ Data should not be specification work. In case of colored products, the values could vary slightly by color.
Recommended
Extrusion Process
Note: The temperature for cable extrusion should be set at the situation of good cable surface performance.
| Zone1 | Zone2 | Zone3 | Zone4 | Neck | Die | Eye |
|---|---|---|---|---|---|---|
| 150 ±10 | 170 ±10 | 180 ±10 | 190 ±10 | 200 ±10 | 210 ±10 | 220 ±10 |
Packaging & Storage
Packaging and storage
1
Storage
- Package: 25kg per bag, Alumni-plastic inner, Kraft paper outside.
- Storage: no rain, no direct sunlight. Dry it at 70℃~80℃ about 4 hours if the material was storage more than 3 months before used.
2
Suggestion for processing
- The compression value of extrusion screw should be 2.5~3.5
- The time of material heated in the barrel should not exceed 30mins, or it maybe decomposed.