Technical Data

Technical Specifications

Typical physical property data, subject to batch test reports.

PropertiesUnitIndexTypical ValueTest method
Tensile StrengthMPa≥15≥24GB/T 1040-2006
Elongation at break%≥150281GB/T 1040-2006
Heat ageing-≥--YHS-UL83-105-2008
Retention at tensile strength%≥75113-
Retention at elongation%≥6584-
Thermal deformation%≤3021GB/T 8815-2008
Low temperature brittleness℃-20PassGB/T 5470-2008
Volume resistivity at 20℃Ω·m≥1.0×10¹²1.2×10¹³GB/T 8815-2008
Dielectric strengthMV/m≥2025GB/T 1408.1-2006
Oxygen index%≥2627GB/T 2406-1993
Densityg/cm³-1.33GB/T 1033.1-2008
Shore hardnessShoreA-90GB/T 2411-2008
Eco-friendly requirements-RoHS&REACH requirementsPass-
Processing Guide

Recommended Processing Parameters

1

  • This product can be processed on extruder with a diameter≥20. The extrusion processing performance is good.
2

  • Extrusion temperature for reference: Zone1 140 Zone2 170 Zone3 180 Zone4 185 Tool 185 Head 185
⚠️ It can be adjusted according to the state of plasticizing.